0
fatal
0
serious
No injury
highest injury
Destroyed
damage

What happened

AAIB synopsis, verbatim

Yak-50, G-YAKK

Conclusion

the AAIB's conclusion, verbatim
Discussion It was clear that the accident had resulted from bursting of G-YAKK's pneumatic system main reservoir. In view of the evidence that the pneumatic system pressure indications had been normal and that the PRV was operating normally it was highly unlikely that overpressure had contributed to the bottle failure, particularly given the slow charge rate of the engine-driven pump. The severe internal corrosion evident included many deep pits that had extended almost to the outer surface. However, it also included a region of drastically reduced wall thickness in the bottom of the bottle, apparently associated with pooling of water at some stage. The evidence suggested that deformation in this thinned area had led to initiation of a crack that had extended rapidly around the bottle. It was therefore concluded that the burst had resulted from fracturing of the bottle at normal pressure due to gross weakening caused by the effects of severe internal corrosion. Inquiries suggested that internal corrosion of the pneumatic system reservoirs was not uncommon, with extensive deep corrosion pitting being found at times. There had been a number of instances where very advanced internal corrosion had been identified because the system had lost pressure after pitting had progressed through the complete wall thickness, creating a pinhole leak. One such bottle that was examined exhibited a sizeable area of internal corrosion and pitting in the region of the drain port. No previous case of a bottle having burst was identified but detailed research has not been possible. Document title It was inevitable that water would be present in a system of this sort, both in liquid form due to condensation and as a vapour. While the water trap would possibly retain much of the water, it appeared probable that the interior of the bottles would be wet for much of the time. It was likely that this environment, with the air present, would oxidise the steel material of the bottles in the absence of adequate internal surface protection. The action of draining the water trap could tend to give the expectation that the system had been drained of water but would in fact have no effect on removing any water present in the bottles. There appeared to be no published or generally accepted standards for inspection or corrosion protection of the bottles. In this situation, given that previous cases of advanced corrosion had occurred, it appeared that the five year interval between overhauls was excessive. Information suggested that annual inspection and proof-pressure testing of high-pressure gas bottles is common industry practice. Previous known cases of failure of this type of bottle due to severe internal corrosion had apparently been relatively benign, as pinholing of the wall by pitting had caused loss of pressure and thus prompted maintenance action and fracturing had not occurred. There was insufficient evidence to establish the reasons for the different failure mode in G-YAKK's case. However, G-YAKK's bottle had almost reached the pit penetration stage and examination of one of the bottles that had previously suffered the more benign failure again found a region of advanced corrosion near the drain port (Figure 10) that could have been close to fracturing. Pooling of water in the bottle had apparently been a factor in both of these failures and no reason was evident as to why such pooling would be unusual. It appeared that small variations in conditions as internal corrosion progressed could cause the fracture mode to occur before a pinhole formed and provided an alert. Document title The failure on G-YAKK was potentially hazardous to the pilot, other personnel and aircraft on the ground and could have been catastrophic had it occurred in flight. Furthermore, the bursting of one of the bottles on the Yak-52, apart from the effects on the aircraft and its systems, could cause major trauma to the rear seat occupant. Additionally, severe injury to maintenance or other personnel would be a distinct possibility if a bottle, fitted to aircraft types with a similar system, burst on the ground. It appeared that the previous failures have led to an expectation that advanced internal corrosion within this type of bottle would be indicated by pinholing and that potentially catastrophic bursting would not occur. As a result, a less scrupulous attitude may have arisen towards preventing, detecting and rejecting corrosion than would be warranted by the potentially catastrophic damage that a high- pressure container of this sort could clearly inflict, should it fracture. It thus appeared possible that significant levels of internal corrosion of this type of bottle fitted to aircraft on the UK Register may be widespread. Although known previous failures had been relatively benign, no evidence was identified to suggest that advanced corrosion would necessarily result in su
In FlarePath for this case

What an account opens