FlarePath
UK AAIB AAIB-1998-TFABT · UK AAIB · Field investigation

Lockheed L1011

South of London Gatwick Airport · 1998-09-30·TF-ABT

Open this case in FlarePathSign inThe record below is free to read. An account opens the recorders, the photographs and the Analyst.
0
fatal
0
serious
No injury
highest injury
Substantial
damage

What happened

AAIB synopsis, verbatim

Lockheed L1011 Tristar, TF-ABT

Conclusion

the AAIB's conclusion, verbatim
Discussion Failure of the duct clearly caused the ECS bay to become pressurised. The door is understood to be capable of carrying a pressure differential of approximately 2 psi. Although a blow out door provides pressure relief at approximately 1.5 psi differential, this is believed to have been designed to accommodate leakage from joints rather than complete duct failure. The normal operating duct pressure is in the region of 20 psi and the flow rate available with all 3 engines supplying the main manifold is considerable. It is likely to have been such that even with the blow-out door open, the available area of its aperture was insufficient to prevent the internal pressure from rising above the 2 psi necessary to fail the main ECS door attachments, once the duct had fractured. Although welding of commercially pure titanium normally results in a slight local hardness increase, a well executed weld should only produce an increase in the range 10 to 25 HV. The weld at the duct fracture location exhibited a much greater hardness increase (45 HV) and would therefore be expected to have had reduced ductility, imparing the fatigue characteristics of the duct. A difference greater than 30 HV compared with the parent material with an associated loss of ductility can indicate that gas contamination has occurred, leading to weld embrittlement. Gas contamination and embrittlement occurs when the weld pool is not sufficiently shielded from atmospheric gases such as oxygen, nitrogen and hydrogen. The blue/purple tint to the weld area adjacent to the fracture is evidence of elevated temperature oxidation; the fact that this feature is only visible in the weld region strongly suggests that it occurred during the weld operation rather than in subsequent service. The geometry produced by the lack of fusion between components at the edge of the weld probably resulted in local stress concentrations, thereby encouraging fatigue growth at that location, although there is no evidence to suggest that similar geometry would not have been present on correctly welded components. The positions of the fatigue origins, on the outside of the main pressure carrying cylindrical section, within the circumference of the mounting collar, are not, however, consistent with the expected effects of the theoretical pressure or thermal cycles (ie the maximum stresses generated by the above loadings would be expected on the inner rather than the outer surfaces at this location). Mounting loads do not pass through the fractured area since the mounting collar attaches the rear part of the failed component to the aircraft structure at a point on the duct aft of the failure plane (Figure 1). Tensile and bending loads acting on the fracture face should have been limited by the presence of the compensator positioned slightly forward of the joint between the failed duct section and the longer section connected to its forward face. It is not therefore immediately obvious which element of the duty cycle created the fatigue stresses leading to the cracking. The material of the ducting has been widely used in this type of application in a number of common aircraft types. There is a history of failures of pneumatic ducting in the regions of welds on more than one aircraft type, so, although the exact mechanism of crack development is not clear in this case, any inadequacy in weld quality could confidently be expected to reduce the life of such a component. The manufacturing date on the data plate of the failed component, preceding as it does the aircraft delivery date by some 5 months, strongly suggests that this was the original component. In this case it would have completed 37,000 hours of operation. This figure is below the fleet average for a type whose earliest examples have been in service for approximately 25 years. It must be assumed that a significant number of ducts of this design are in service having completed substantially more flight cycles than this failed component. Emergency procedures The aircraft is normally operated with the isolation valves, situated in the main manifold, in the open position. Once failure of any ECS ducting occurs, airflow will continue through the failed duct, as long as at least one engine continues to supply bleed air to the manifold. The position of the failure on TF-ABT allowed the leaking air to activate the adjacent heat detector causing the relevant warning (zone A overheat) to operate on the flight engineer's panel. His action in selecting No 1 pack 'off' closed the No 1 ECS flow control valve, successfully shutting off the bleed air to the failed duct.
In FlarePath for this case

What an account opens

The Explorer account is free and reads the whole record. The recorders, the Analyst and the Casebook are the paid plans.